How to Tig Weld coke cans with a miller dynasty 200dx and an Everlast powertig 250ex, good tig welding settings for thin aluminum are 60 pps, 30% t and 20% background current. 60% ac balance, and 90hz frequency worked out ok.
Low amperage starts on both machines allow arc starts with no holes blown.

Click the Watch Stuff menu in the top bar to view more videos, or get a pantload more info at http://www.weldingtipsandtricks.com/.



Click here to subscribe to my Video of the Week!


2 Responses to Tig Welding Aluminum Coke Cans with Everlast Powertig 250ex and Miller Dynasty 200dx

  1. Logan McCullough on September 18, 2011 at 12:52 PM

    Hey Jody, What should I set the amperage on for this. With the dynasty. Sorry if this is a dumb question, I just started tig welding awhile ago.

    • Mike on December 12, 2012 at 2:39 PM

      You can see the amperage setting at 2:17 on the video. 49 AMPS if using the other pulse settings he discusses.

      That’s NOT 49 AMPS average… because it’s on 30% of the time, with only 20% of that amperage being used during the remaining 70% of the pulse cycle…