Short circuit MIG with 7525 gas downhill. Working with different sized wire, thicknesses and alternating with cold rolled and hot rolled steel.
Short circuit MIG with 7525 gas downhill. Working with different sized wire, thicknesses and alternating with cold rolled and hot rolled steel.
This is part 2 of TIG Aluminum with Argon and Argon Helium mix on aluminum. Using a Swag Offroad portaband stand to section the welds.
TIG welding aluminum lap joints one with argon and one with argon helium mix. No fancy mixer just a simple Y setup.
Welding some thin (1 mm thick) aluminum today. Gonna be using 2 machines one maxes out at 250 and the other at 400 hertz and comparing the results.